Abstract
In the present study, bead-on-plate specimens of 1-mm sheets of austenitic and duplex stainless steels were fabricated by laser penetration welding with a 2.5-kW CW Nd:YAG laser. The galvanic corrosion behavior of laser-weldment (LW) against as-received (AR) specimens with an area rato of 1:1 in 3.5% NaCL solution was studied by means of a zero-resistance ammeter. The free corrosion potentials of as-received specimens were found to be considerably higher than those of laser weldments, indicating that the weldments are more active and always act as anodes. The ranking of galvanic current densities (IG) of the couples in ascending order is: AR S31603-LW S31603 < AR S31803-LW S31803 < AR S32760-LW S32760 < AR S30400-LW S30400. For the galvanic couple between AR S30400 and LW S30400, the IG is the highest (78.6 nA/cm2) because large amount of δ-ferrite in the weld zone acts as active sites. On the other hand, the IG of the galvanic couple between AR S31603 and LW S31603 is the lowest (-26 nA/cm2) because no δ-ferrite is present after laser welding. The recorded IG of all couples revealed constantly low values (in the rnage of nA/cm2) and sometimes stayed negative, which indicated polarity reversal.
© (2004) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Chi-Tat Kwok, Siu Lung Fong, Fai Tsun Cheng, and Hau-Chung Man "Investigation of galvanic corrosion in laser-welded stainless steel sheets", Proc. SPIE 5662, Fifth International Symposium on Laser Precision Microfabrication, (8 October 2004); https://doi.org/10.1117/12.596319
Lens.org Logo
CITATIONS
Cited by 2 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Corrosion

Laser welding

Molybdenum

Barium

Chromium

Continuous wave operation

Nd:YAG lasers

RELATED CONTENT

2 kW cw Nd:YAG laser surface hardening
Proceedings of SPIE (April 04 1997)
Microtribiology and self-lubrication microsystems
Proceedings of SPIE (September 01 1998)
Laser reflow plastic ball grid array
Proceedings of SPIE (February 25 2002)

Back to Top