Paper
7 March 2014 Low-loss titanium-dioxide strip waveguides by atomic layer deposition
M. Roussey, M. Häyrinen, A. Säynätjoki, V. Gandhi, L. Karvonen, P. Stenberg, M. Kuittinen, S. Honkanen
Author Affiliations +
Proceedings Volume 8982, Optical Components and Materials XI; 89820E (2014) https://doi.org/10.1117/12.2038912
Event: SPIE OPTO, 2014, San Francisco, California, United States
Abstract
In this paper we describe an approach to reduce the propagation loss in titanium dioxide strip waveguides. We achieved to reduce losses down to 2.4 dB/cm in 1 μm-wide waveguide at λ=1550 nm.
© (2014) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
M. Roussey, M. Häyrinen, A. Säynätjoki, V. Gandhi, L. Karvonen, P. Stenberg, M. Kuittinen, and S. Honkanen "Low-loss titanium-dioxide strip waveguides by atomic layer deposition", Proc. SPIE 8982, Optical Components and Materials XI, 89820E (7 March 2014); https://doi.org/10.1117/12.2038912
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Waveguides

Titanium dioxide

Atomic layer deposition

Wave propagation

Polarization

Light wave propagation

Scanning electron microscopy

RELATED CONTENT

ALD-tuned titanium dioxide nanophotonics
Proceedings of SPIE (June 01 2015)
High-power laser testing of 3D meta-optics
Proceedings of SPIE (November 14 2013)
Application of atomic layer deposition in nanophotonics
Proceedings of SPIE (March 08 2014)
Compact and efficient couplers for silicon slot waveguides
Proceedings of SPIE (February 02 2012)

Back to Top